Adhesion of Rough Solids
Computational Tribology

Some open problems in adhesion (of rough surfaces)

30.01.2018 tribonet 413 Views

By M.Ciavarella, A. Papangelo. Politecnico di BARI, Italy. Adhesion for ‘‘soft’’ bodies shows instabilities like in the simple case of a single sinusoid even in the so called JKR regime (Johnson 1995) which leads to […]

Tribology News

White etching cracks

29.01.2018 tribonet 445 Views

Today, bearing failure due to rolling contact fatigue is generally a rare occurrence, and the final achieved service life of rolling bearings is usually well in excess of the calculated rating life. There are instances, […]

cartilage
Bio Tribology

Cartilage tribology: Slip sliding away

22.01.2018 tribonet 497 Views

Research sheds light on friction, lubrication and wear in cartilage 11:25 a.m., Aug. 24, 2015–Osteoarthritis, which affects some 27 million people in the U.S. alone, occurs when the protective cartilage on the ends of bones […]