An Algorithm Helps Protect Mars Curiosity’s Wheels

Related image

There are no mechanics on Mars, so the next best thing for NASA’s Curiosity rover is careful driving.

A new algorithm is helping the rover do just that. The software, referred to as traction control, adjusts the speed of Curiosity’s wheels depending on the rocks it’s climbing. After 18 months of testing at NASA’s Jet Propulsion Laboratory in Pasadena, California, the software was uploaded to the rover on Mars in March. Mars Science Laboratory’s mission management approved it for use on June 8, after extensive testing at JPL and multiple tests on Mars.

Even before 2013, when the wheels began to show signs of wear, JPL engineers had been studying how to reduce the effects of the rugged Martian surface. On level ground, all of the rover’s wheels turn at the same speed. But when a wheel goes over uneven terrain, the incline causes the wheels behind or in front of it to start slipping.

This change in traction is especially problematic when going over pointed, embedded rocks. When this happens, the wheels in front pull the trailing wheels into rocks; the wheels behind push the leading wheels into rocks.

Traction control testingA “scarecrow” rover at NASA’s JPL drives over a sensor while testing a new driving algorithm. Engineers created the algorithm to reduce wheel wear on the Mars Curiosity rover. Image Credit: NASA/JPL-Caltech

In either case, the climbing wheel can end up experiencing higher forces, leading to cracks and punctures. The treads on each of Curiosity’s six wheels, called grousers, are designed for climbing rocks. But the spaces between them are more at risk.

“If it’s a pointed rock, it’s more likely to penetrate the skin between the wheel grousers,” said Art Rankin of JPL, the test team lead for the traction control software. “The wheel wear has been cause for concern, and although we estimate they have years of life still in them, we do want to reduce that wear whenever possible to extend the life of the wheels.”

The traction control algorithm uses real-time data to adjust each wheel’s speed, reducing pressure from the rocks. The software measures changes to the suspension system to figure out the contact points of each wheel. Then, it calculates the correct speed to avoid slippage, improving the rover’s traction.

During testing at JPL, the wheels were driven over a six-inch (15-centimeter) force torque sensor on flat terrain. Leading wheels experienced a 20 percent load reduction, while middle wheels experienced an 11 percent load reduction, Rankin said.

Traction control also addresses the problem of wheelies. Occasionally, a climbing wheel will keep rising, lifting off the actual surface of a rock until it’s free-spinning. That increases the forces on the wheels that are still in contact with terrain. When the algorithm detects a wheelie, it adjusts the speeds of the other wheels until the rising wheel is back into contact with the ground.

Image result for Mars Curiosity

Technicians look over the MSL Curiosity during inspections at the Jet Propulsion Laboratory in Pasadena, Calif. Phot credit: NASA

Rankin said that the traction control software is currently on by default, but can be turned off when needed, such as for regularly scheduled wheel imaging, when the team assesses wheel wear.

The software was developed at JPL by Jeff Biesiadecki and Olivier Toupet. JPL, a division of Caltech in Pasadena, manages the Curiosity mission for NASA.

Andrew Good on 29th June 2017
Jet Propulsion Laboratory, Pasadena, California
[email protected]v

Source: Jet Propulsion Laboratory News

tribonet
About tribonet 312 Articles
Administration of the project

Be the first to comment

Leave a Reply

Your email address will not be published.


*


This site uses Akismet to reduce spam. Learn how your comment data is processed.