• Welcome to tribonet! Our goal is to popularize and raise awareness of tribology and its branches among students, engineers, researchers and enthusiasts. Latest news and developments, updates and upcoming events are gathered on tribonet. Everyone is welcome to contribute by sharing “popular science” articles, news, or updates and related codes and materials or contribute to tribology Wikipedia .

  • Please log-in or register to download this file

  • Download Info

    • Categories: Contact Mechanics
    • File size: 1.22 MB
    • Author: deepakiitp
    • Updated: 22.05.2017
    • Rating: (0)
      Thanks for rating!
    • Views: 537
    • Downloads: 57
  • This work demonstrates the importance of summit parameters for an anisotropic Gaussian rough surface. It is shown that lay direction may significantly affect the running-n wear process.