Method to view the Crystal Structure of Metals

metal crystal

Method uses readily available tools to quickly determine materials’ properties.

Researchers at MIT and elsewhere have developed a new combination of methods that can provide detailed information about the microstructure of polycrystalline metals.

Such materials — composed of a random matrix of multiple small crystals rather than one single large crystal — are widely used for such applications as nuclear reactors, civil infrastructure, and aircraft. However understanding the details of their crystal structure and the boundaries between the crystal areas has been difficult.

The new findings are published in the journal Nature Computational Materials, in a paper by Matteo Seita, an MIT postdoc; Michael Demkowicz, a professor of materials science and engineering; Christopher Schuh, the Danae and Vasilis Salapatas Professor of Metallurgy, and five others.

“This is a unique combination of different technologies,” Seita explains. The new approach he and the team developed addresses “one of the most common problems in materials science: How do we quantify the characteristics of materials in a high-throughput fashion?”

Some techniques offer a great deal of detail about structures, but they take time to carry out and can’t reveal rapid changes within the material. Others work rapidly but provide much less structural detail, and still other methods provide both spatial and temporal detail but are prohibitively expensive or only available in limited places. The new combination of techniques, Seita says, can help resolve these limitations by providing fast, high-resolution, and low-cost imaging of the materials.

In polycrystalline metals, which are composed of many small crystal grains, it is important to know the location, dimensions, angles of contact, and other characteristics of the different grains making up the material. In particular, the interfaces between the crystal grains, called grain boundaries, “happen to be critical,” Seita says, “to many individual properties of the material — its strength, radiation tolerance, hardness, electrical resistance, and so on — but they are very difficult to characterize experimentally, because they are very complex.”

There are five basic characteristics about these grain boundaries that researchers would like to be able to quantify, but most tools for studying the materials can only yield some subset of two or three of those. One method for getting all five characteristics at once is  high-energy synchrotron radiation, which is only available in a few facilities that are expensive and tend to be oversubscribed.

“Our solution was to try to create a very simple technology that can be used by anyone, in their own lab, using software and hardware that are easily available,” Seita says. And that’s what they achieved, using a combination of two existing methods — optical microscopy and electron microscopy.

“We take two different datasets and combine them using our numerical image analysis,” he explains. To do so, they used sheets of polycrystalline metal foil, which were thin enough that single grains could be seen from both sides. They then took optical microscope images of the foil from one side, flipped the sheet over, and imaged the other side, and used software to connect the grain boundaries from one side to the other. From that, he says, “We can reconstruct the 3-D orientation of these grain boundaries.”

Then, that information is combined with electron microscope images that describe the actual pattern of atoms within the grains, showing the orientation of the individual crystal lattices within each grain — and how they relate to those of adjacent grains. The combined information provides all five characteristics of the grain boundaries in the metal foils.

“The beauty of this is that it’s high-throughput technology,” Seita says. “On one sample, we can measure up to 500 grain boundaries or so, and can build up datasets rapidly. And it’s nondestructive,” unlike existing methods that consume the sample in the process. That means the sample can then be subjected to other tests, for example tests of mechanical or electrical properties, whose results can be compared with the data about the grain boundaries.

The new methodology, Seita says, “is very versatile, so many groups out there can use it.” What’s more, though the initial tests were done with polycrystalline metals, the technique “is materials agnostic,” and could be applied to insulators or semiconductors as well as metals. “We can test for different kinds of properties and build up large datasets,” he says, and ultimately use that data to predict the characteristics of new polycrystalline materials.

“We can figure out what kind of grain boundaries we want to have” for a material being designed for a particular application, “and figure out how to make a material with those grain boundaries.” Manipulating the characteristics of these grain boundaries, by modifying the material to increase their abundance or relative orientations, can produce significant changes in the material’s property. So, for example, the technique might be used to figure out how to reduce the rate of corrosion of metals exposed to harsh environments, such as oil or gas drilling equipment, he says.

The method combines optical microscopy techniques (left, in pink) with electron backscatter diffraction (right, in green) to measure characteristics of the boundaries between crystal grains, which help determine the material’s overall properties.
The method combines optical microscopy techniques (left, in pink) with electron backscatter diffraction (right, in green) to measure characteristics of the boundaries between crystal grains, which help determine the material’s overall properties. Image: Matteo Seita

This work is “an inspiring step forward in rapid, data-rich characterization of the structure of crystalline materials,” says Brad Boyce, a distinguished member of the technical staff at Sandia National Laboratories in New Mexico, who was not involved in this research. “Grain boundaries, which are interfacial disruptions in the crystalline lattice of polycrystals, influence a wide range of material phenomena ranging from how the material deforms to the electrical resistivity … yet materials scientists possess a limited range of techniques to explore the grain boundary character.”

Now, with this new technique, Boyce says, “I am excited to see how this work will inspire further developments that provide rapid, high-throughput characterization, especially techniques that can be used to decipher local grain boundary character below the spatial resolution limits of optical microscopy.”

The team also included Marco Volpi and Maria Vittora Diamanti of the Polytechnic University of Milan, in Italy; Srikanth Patala at North Carolina State University; and Ian McCue and Jonah Erlebacher at Johns Hopkins University, in Baltimore. The work was supported by the U.S. Department of Energy, the National Science Foundation, and the MISTI Seed Fund.

David L. Chandler on 6th of July 20163

MIT News Office

Source: MIT News

tribonet
About tribonet 313 Articles
Administration of the project

Be the first to comment

Leave a Reply

Your email address will not be published.


*


This site uses Akismet to reduce spam. Learn how your comment data is processed.