Laser-Cooled Ions Help to Understand Friction

doppler laser cooling technique

Physics supports biology: Researchers from PTB have developed a model system to investigate friction phenomena with atomic precision

Friction: what you want from car brakes, otherwise rather a nuisance. In any case, it is useful to know as precisely as possible how friction phenomena arise – and not only on the macroscopic scale (like in mechanical engineering), but also on the microscopic scale (i.e. in areas such as biology and nanotechnology). It was previously difficult to study friction where everything is as small as an atom and where, in addition, non-linear effects prevail. Scientists from the QUEST Institute at the Physikalisch-Technische Bundesanstalt (PTB) have now presented a model system which allows the investigation of atomic-scale friction effects and friction dynamics that are similar to those taking place, e.g., in proteins, DNA strands and other deformable nanocontacts. This model system consists of laser-cooled ions, which arrange themselves in so-called Coulomb crystals. With these, the researchers have carried out experiments and numerical simulations and obtained new fundamental findings on friction processes in atomic systems. They have now presented their results in the scientific journal “Nature Communications”.

http://www.ptb.de/cms/fileadmin/_processed_/csm_Grafik-Reibung_d81315f02d.jpg

a) Schematic representation of the experiment: 30 ytterbium ions are trapped in a linear radio-frequency trap. Laser 1 irradiates the whole crystal and makes it fluoresce. This light is collected by means of a high-resolution lens and imaged onto a camera. Laser 2 is aligned to one of the chains, so that a differential light force acts between them. b) Schematic representation of the model system: The ions interact with each other and with the trap via springs. Due to a structural defect, spacing a1 and a2 are mismatched. (Figure: PTB)

Hardly any other physical phenomenon is of such importance in nature and our technological environment as friction phenomena are: without static friction, even our everyday life would not work. Static friction ensures that things do not slip out of our hands when we grab them and that we can firmly stand on the ground. Without friction, it would be impossible to get a vehicle into motion since the wheels would simply spin. These are positive aspects of friction, but there are also negative ones: without friction, there would be no cracks due to earthquakes, machine parts would not wear down, etc.

Most macroscopic objects have a rough texture from an atomic view point. Even if they feel smooth to the touch, they exhibit asperities. Strictly speaking, two objects never lie directly on top of each other, but only touch each other at these asperities. The atomic lattice structure therefore plays no role in this interaction. This is quite different for objects on the atomic scale, like nanomachines or biomolecules. “Here, atomically smooth surfaces touch each other. The surface therefore also plays a role and must be taken into account in model calculations”, explains PTB physicist Tanja E. Mehlstäubler. “These models also explain fascinating phenomena such as superlubricity, where static friction becomes nearly non-existent. It occurs when two crystalline surfaces are incommensurate to each other. This means that the ratio of the lattice spacings of the sliding surfaces is irrational. This leads to there being no place where the two surfaces are an exact match for each other.”

There are thus enough reasons to precisely measure friction at the nanoscale and to investigate its dynamics. When it comes to measuring friction, a powerful instrument already exists, namely the friction force microscope. The second point is more complex: “Direct experimental access to the dynamics of a friction system is nearly impossible. Model systems in which the atoms are easily controlled – both temporally and spatially – are therefore indispensable. This allows us to investigate them”, explains Mehlstäubler. Such a system has now been presented by the scientists from PTB, together with their partners from Sydney: ytterbium ions kept in an ion trap are cooled by means of lasers to such an extent (down to a few millikelvins) that they form a crystal consisting of two chains. The ions arrange themselves in such a way that the nearest neighbor is always as far away as possible. This structure is called a zigzag.

Image result for laser cooled ions

Laser (Doppler) Cooling (Source: NPL)

Two such ion chains are a very accurate representation of the two partners of a friction process – and they are easy to observe very precisely: when ytterbium ions are irradiated with light whose frequency is close to their resonant frequency, they begin to fluoresce. “We are thus able to observe the individual atomic particles in their motion through our imaging optics”, adds Jan Kiethe, a physicist at PTB and the main author of the study. A transition between two different phases, which was caused by the presence of a structural lattice defect, has been observed and analyzed here. In one of the regimes, static friction is the main actor in the transport dynamics; in the other regime, it is sliding friction.

The dynamics of the ion chains is comparable to that of molecule chains such as those occurring in DNA. With their now published work, the scientists have created a physical model system which will make it possible to investigate the complex dynamics of friction in 1D, 2D and 3D systems with atomic precision. Moreover, this model system has paved the way for the investigation of transport phenomena in the quantum regime.

This project was supported by the Deutsche Forschungsgesellschaft (grant ME 3648/1-1), the German Academic Exchange Service (Deutscher Akademischer Auslandsdienst – DAAD) and the EPSRC “National Quantum Technology Hub in Networked Quantum Information Processing”.

Erika Schow on 13th of July 2017

Contact:

Dr. Tanja E. Mehlstäubler, QUEST Institute at PTB, phone: +49 (0)531 592-4710,
E-mail: [email protected]

Scientific publication

J. Kiethe, R. Nigmatullin, D. Kalincev, T. Schmirander, T. E. Mehlstäubler: Probing nanofriction and Aubry-type signatures in a finite self-organized system. Nature Communications 8: 15364 (2017), DOI: 10.1038/ncomms15364

Source: PTB

tribonet
About tribonet 313 Articles
Administration of the project

Be the first to comment

Leave a Reply

Your email address will not be published.


*


This site uses Akismet to reduce spam. Learn how your comment data is processed.