Low-temperature steel hardening – a new way

13.04.2018 tribonet 189 Views
EU-funded researchers developed a novel process for surface hardening of stainless steel that ensures high hardness with extraordinary corrosion and fatigue resistance properties. Stainless steel is the material of choice in various industries where corrosion […]