wear particle
Computational Tribology

Adhesive wear model: particle by particle

23.07.2017 tribonet 1,415 Views

10.07.17 – An EPFL study has deepened our understanding of the fine particles produced by adhesive wear. This breakthrough could lead to cost savings and environmental benefits. Adhesive wear occurs when two surfaces – such […]