Advanced Materials

Droplet friction is similar to solid friction

21.11.2017 tribonet 361 Views
Researchers of the Max Planck Institute for Polymer Research have investigated friction of liquid droplets on surfaces. A larger force is needed to set in motion stationary droplets than to keep moving droplets in motion. […]