Controllable surface texture
Advanced Materials

A multifunctional, multiscale, reconfigurable surface

31.07.2018 tribonet 68 Views

Composite surface has features that can move microparticles, mix droplets, repel biofilms and more [embedded content] An international team of researchers, led by Harvard University, have developed a dynamic surface with reconfigurable topography that can […]