graphene
Advanced Materials

How sticky tape makes graphene

09.03.2018 tribonet 89 Views

Scientists at UCL have explained for the first time the mystery of why adhesive tape is so useful for graphene production. The study, published in Advanced Materials, used supercomputers to model the process through which […]