Benefits of Hybrid Bearings in Severe Conditions

03.07.2017 tribonet 276 Views
Hybrid bearings, i.e., bearings with steel rings and bearing grade silicon nitride (Si3N4) rolling elements, have been increasingly used in applications operating in challenging environments [1-4] such as high-speed, oil-free air conditioning and refrigeration compressors, […]