The Defence Science and Technology Laboratory (Dstl) in Porton Down has announced it has revolutionized the production of titanium by reducing the 40 stage process down to just two steps and potentially halving the cost.

Titanium is as strong as steel and half the weight – but around ten times the cost. It is notoriously difficult and expensive to make which limits its wider use.

Defence Secretary Gavin Williamson said:

“Our Armed Forces use titanium in everything from cutting-edge nuclear submarines and fighter jets through to life-changing replacement limbs – but production time and costs mean we haven’t always used it. This ground-breaking method is not only faster and cheaper but could see a huge expansion of titanium parts and equipment throughout the military. It is a clear example of how our world-class scientists are working behind the scenes to help our Armed Forces as well as bringing prosperity and security to Britain.”

Titanium’s high strength, light weight and corrosion resistance sees it widely used in defence, in military aircraft and submarines, but its high production costs make it difficult to justify in all but essential areas.

Dstl has invested almost £30,000 in the new research project carried out in the Department of Materials Science and Engineering at the University of Sheffield, which led to the development of the new ground-breaking manufacturing process.

The announcement comes as Dstl supports the Defence Procurement Research Technology and Exportability (DPRTE), which takes place March 27.

The pioneer of this revolutionary technique, Dr Nick Weston, from the University, said:

“FAST-forge is a disruptive technology that enables near net shape components to be produced from powder or particulate in two simple processing steps. Such components have mechanical properties equivalent to forged product. For titanium alloys, FAST-forge will provide a step change in the cost of components, allowing use in automotive applications in automotive applications such as powertrain and suspension systems.”

The process gets its name from the Field Assisted Sintering Technology, which is used to produce a preformed billet, which are close to the size and shape of the finished part (near net shape) directly from titanium alloy powders, before a single hot forging operation produces the final part.

So far, small-scale trials have been carried out, but a new large-scale fast furnace facility jointly funded by Dstl and Kennametal Manufacturing (UK) Ltd has been built and will enable larger components to be produced for testing.

Matthew Lunt the Principal Scientist for Materials Science at Dstl said:

“We’re really excited about this innovation, which could cut the production cost of titanium parts by up to 50%. With this reduction in cost, we could use titanium in submarines, where corrosion resistance would extend the life, or for light-weight requirements like armoured vehicles.”

Further information about the FAST-forge process can be found here.

A Case Study describing early developments can be found here.

26th of March 2018Sheffi

The University of Sheffield News

Source: University of Sheffield

tribonet
About tribonet 313 Articles
Administration of the project

Be the first to comment

Leave a Reply

Your email address will not be published.


*


This site uses Akismet to reduce spam. Learn how your comment data is processed.