Argonne Embraces Concept of "in operando" Formation of Carbon-based Tribofilms
Earlier this month, tribologists and physicists at the U.S. Department of Energy (DOE) Argonne National Laboratory published news of their (self-described) “self-healing diamond-like carbon coating [that] could revolutionize lubrication” in the journal Nature. The researchers […]