Concrete strength is determined by internal friction

03.10.2017 tribonet 1,313 Views

Cement materials, including cement paste, mortar, and concrete, are the most widely manufactured materials in the world. Their carbon footprint is similarly hefty: The processes involved in making cement contribute almost 6 percent of global […]

Featured Video

Recent Comments

  • MAcostaTribonet on Contact Pressure For Rough Surfaces: A Tutorial
  • MAcostaTribonet on Contact Pressure For Rough Surfaces: A Tutorial
  • tribonet on Contact Pressure For Rough Surfaces: A Tutorial
  • MAcostaTribonet on Contact Pressure For Rough Surfaces: A Tutorial

Popular Wikis

  • Hertzian contact equations for elliptical, spherical and cylindrical contacts
  • Hertzian contact theory
  • Wear
  • Fretting, fretting corrosion and fretting mechanisms
  • Pin on Disk Test
  • Fatigue Wear
  • Reynolds Equation: Derivation and Solution
  • Galling
  • Bio-Inspired Surface Replication
  • Nanotribology
  • Superlubricity
  • Elastohydrodynamic Lubrication (EHL): Theory and Definition
  • Friction
  • Coefficient of Friction
  • Oil Viscosity Index and Viscosity Temperature Relation
  • Adhesive Wear
  • Abrasive Wear
  • Corrosive Wear
  • Laws of Friction
  • Wear Particles
  • What is EHD film thickness?
  • Tribochemistry
  • Archard Wear Equation
  • Engine Bearing
  • Pressure-Viscosity Coefficient and Characteristics of Lubricants
  • Tribometers
  • Elastic Deformation
  • Greenwood and Williamson Contact Model
  • Hydrodynamic Lubrication (HL): Theory and Definition
  • Power Spectral Density of Rough Surfaces
  • Plastic Deformation at Microscale
  • Generalized Reynolds Equation: Derivation
  • Analytical Solution of Reynolds Equation: Grubin's Approximation
  • Grease
  • Tribology
  • Four Ball Tester
  • What Are Lubricants?
  • Coefficients of Kinetic and Static Friction
  • Boundary Lubrication
  • Friction Coefficient Tables in Air and Vacuum
  • Triboelectricity
  • Environmentally Acceptable Lubricants
  • Rolling Contact Fatigue
  • Triboluminescence

Search in Tribology Wikipedia


Newsletter Sing Up

Articles in Pictures

  • Tribology mechanisms
  • Wear Model
  • vacuum oil flow
  • recuperative breaking
  • tribology to extend machine lifetime
  • Atomic scale friction on graphene
  • electrostatic charge

More to Read

  • Image result for summer and winter tires

    Tribology and the Human Evolution

    12.08.2019 997 Views
    Tribology, not a common household word, is the science of wear, friction, and lubrication, studying how interacting surfaces behave in relative motion. Tribology does not work in isolation but affects a multitude of other fields [...]
  • Can we please get rid of the toxic copper in brake pads?

    21.12.2020 1,142 Views
    Whatever humanity does today, it does it on a very large scale. And the consequences are large as well! In the automotive area, I was clearly aware of CO2 emissions and global warming issues. A [...]
  • recycling plastic trash

    Making Lubricants From Plastic Waste

    30.03.2020 519 Views
    Single-use plastics have a bad reputation for contributing to the earth’s environmental and pollution issues. With the world’s ever-vigilant focus on protecting the environment, society is determined to halt the use of single-use plastics, such [...]
  • Argonne Embraces Concept of "in operando" Formation of Carbon-based Tribofilms

    23.08.2016 471 Views
    Earlier this month, tribologists and physicists at the U.S. Department of Energy (DOE) Argonne National Laboratory published news of their (self-described) “self-healing diamond-like carbon coating [that] could revolutionize lubrication” in the journal Nature.  The researchers [...]
  • Electric Vehicles

    Tribology Trends and Challenges in Electric Vehicles: Short Summary

    14.09.2020 1,005 Views
    Electric vehicles, while often considered a new phenomenon, have existed since the 1800s. At that point in time, electric vehicles outnumbered gasoline powered vehicles for many reasons. Electric vehicles did not have the same vibration, [...]
  • Sign Up
  • About Us
  • Contacts
  • Contributing Writers
  • Advertising
  • Privacy Policy
  • Disclaimer
  • Writing Articles
  • Downloads

© 2016-2021 tribonet

Skip to toolbar
  • Log In
  •   Register