Superlubricity by means of repulsive van der Waals forces

06.04.2016 Dr. Aydar Akchurin 808 Views

Superlubricity, a state of low friction (<0.001), can be achieved by different mechanisms. The structural superlubricity occurs, if the crystal lattices of the contacting bodies are incommensurate. Nano-scrolls may act as a bearing and may […]

Featured Video

Recent Comments

  • MAcostaTribonet on Contact Pressure For Rough Surfaces: A Tutorial
  • MAcostaTribonet on Contact Pressure For Rough Surfaces: A Tutorial
  • tribonet on Contact Pressure For Rough Surfaces: A Tutorial
  • MAcostaTribonet on Contact Pressure For Rough Surfaces: A Tutorial

Popular Wikis

  • Hertzian contact equations for elliptical, spherical and cylindrical contacts
  • Hertzian contact theory
  • Wear
  • Fretting, fretting corrosion and fretting mechanisms
  • Pin on Disk Test
  • Fatigue Wear
  • Reynolds Equation: Derivation and Solution
  • Galling
  • Bio-Inspired Surface Replication
  • Nanotribology
  • Superlubricity
  • Elastohydrodynamic Lubrication (EHL): Theory and Definition
  • Friction
  • Coefficient of Friction
  • Oil Viscosity Index and Viscosity Temperature Relation
  • Adhesive Wear
  • Abrasive Wear
  • Corrosive Wear
  • Laws of Friction
  • Wear Particles
  • What is EHD film thickness?
  • Tribochemistry
  • Archard Wear Equation
  • Engine Bearing
  • Pressure-Viscosity Coefficient and Characteristics of Lubricants
  • Tribometers
  • Elastic Deformation
  • Greenwood and Williamson Contact Model
  • Hydrodynamic Lubrication (HL): Theory and Definition
  • Power Spectral Density of Rough Surfaces
  • Plastic Deformation at Microscale
  • Generalized Reynolds Equation: Derivation
  • Analytical Solution of Reynolds Equation: Grubin's Approximation
  • Grease
  • Tribology
  • Four Ball Tester
  • What Are Lubricants?
  • Coefficients of Kinetic and Static Friction
  • Boundary Lubrication
  • Friction Coefficient Tables in Air and Vacuum
  • Triboelectricity
  • Environmentally Acceptable Lubricants
  • Rolling Contact Fatigue
  • Triboluminescence

Search in Tribology Wikipedia


Newsletter Sing Up

Articles in Pictures

  • control friction in a bearing
  • The Forbidden City
  • gecko
  • Static friction
  • glassy carbon
  • Image result for machine learning and oil analysis
  • cat1
  • cartilage
  • C:\Users\Melanie\AppData\Local\Microsoft\Windows\INetCache\IE\3KSJXYN2\Tokay_foot[1].jpg

More to Read

  • SEM image Boron rich carbide

    High Hardness Boron Rich Boron Carbide is Synthesized using CVD

    18.05.2020 376 Views
    Hardness is a material’s resistance to plastic deformation and this property is widely used to rank materials for various engineering applications. Hard materials can be used for cutting, drilling. Hardness frequently correlates with wear resistance [...]
  • White etching cracks

    29.01.2018 3,951 Views
    Today, bearing failure due to rolling contact fatigue is generally a rare occurrence, and the final achieved service life of rolling bearings is usually well in excess of the calculated rating life. There are instances, [...]
  • Triboelectric generator

    Generating Electricity From Snowfall

    17.06.2019 373 Views
    It is interesting to know that researchers from the University of California, Los Angeles (UCLA) have come up with an innovative device that can generate electricity from the snow we are all familiar with. Nothing [...]
  • Space Fabric folded over

    'Space Fabric' Links Fashion and Engineering

    11.07.2017 1,447 Views
    Raul Polit Casillas grew up around fabrics. His mother is a fashion designer in Spain, and, at a young age, he was intrigued by how materials are used for design. Now, as a systems engineer [...]
  • wave energy

    Triboelectricity to collect wave power

    01.06.2017 1,583 Views
    Nature provides three sources of energy for free: sunlight, air and gravity. Solar and wind power are increasingly exploited, gravity less so. Hydraulic power plants harvest energy from flowing rivers. Tidal energy can be gathered [...]
  • Sign Up
  • About Us
  • Contacts
  • Contributing Writers
  • Advertising
  • Privacy Policy
  • Disclaimer
  • Writing Articles
  • Downloads

© 2016-2021 tribonet

Skip to toolbar
  • Log In
  •   Register