Cartilage Lubrication
Cartilage degeneration is due to osteoarthritis (OA) which is commonly seen in aging populations. This degeneration occurs due to the deterioration of the mechanical and tribological properties of articular cartilage (AC), primarily caused by lubrication failure. Understanding the causes of...