Polymer material produced by a 3-D printer includes soft, flexible material (clear or lighter tone) with particles of hard material (black) embedded, in predetermined arrangements. When the material is compressed, its surface become bumpy in a pattern determined by the hard particles.
Advanced Materials

MIT: surface with reconfigurable texture developed

27.10.2017 tribonet 290 Views
Polymer material produced by a 3-D printer includes soft, flexible material (clear or lighter tone) with particles of hard material (black) embedded, in predetermined arrangements. When the material is compressed, its surface become bumpy in […]