Alloy Strength is Improved by Tiny Additions

Nanoparticles improve the strength of metallic alloys.

Superalloys are the wonder materials of metallurgy. By fine-tuning their composition, scientists can increase mechanical strength and improve resistance to corrosion and high-temperature shape changes. A*STAR researchers have shown that adding nanoparticles can make these materials even stronger.

Inconel 625 is a superalloy that is 55-70 per cent nickel with added chromium, molybdenum, iron, niobium-tantalum, plus trace amounts of numerous other metals. Inconel 625 is used in industrial marine applications because of its high corrosion-fatigue strength, tensile strength and resistance to chloride-ion stress-corrosion cracking.

Guijun Bi and co-workers from A*STAR’s Singapore Institute of Manufacturing Technology and Institute of Materials Research and Engineering have reinforced Inconel 625 using titanium diboride nanoparticles. The improved superalloy is fabricated by a sophisticated technique known as laser-aided additive manufacturing.

nanoparticles

Adding nanoparticles improves the properties of superalloy components created using laser-aided additive manufacturing. © 2017 A*STAR Singapore Institute of Manufacturing Technology

Additive manufacturing is a class of fabrication methods that can create full-scale components by building them up one layer at a time. 3D printing is one well-known example, but for metals, high-power lasers are typically needed. One such method is laser-aided additive manufacturing, a novel additive manufacturing technology which can be utilized for 3D printing, surface modification and repair. It works by applying a laser beam as heat source, with the additive materials melted and deposited on to the surface layer by layer.

“We show that adding nanoparticles to the metal base material is an effective way to tailor the material with significantly improved physical, thermal and mechanical properties, as well as excellent performance in terms of wear and corrosion resistance,” explains Bi.

Bi and the team mixed and ground together an Inconel 625 alloy powder and a titanium diboride powder with particles approximately 58 nanometers in size. Their additive manufacturing system comprised a powder nozzle on a six-axis robot along with the output from a high-power fiber laser. In this way, they were able to create one-millimeter thick layers of their material on a carbon steel substrate, which they built up into a rectangular block of 120 × 70 × 10 millimeters.

Analysis of their sample indicated that the titanium diboride nanoparticles mainly aggregated at boundaries between crystalline grains of the Inconel 625. Thus, the titanium diboride acted to reinforce the grain boundary. Mechanical testing of the sample demonstrated a significantly increased material strength, relatively high micro-hardness and good abrasive resistance.

“We hope to develop this approach and explore new composite materials reinforced with nanoparticles for additive manufacturing” says Bi.

The A*STAR-affiliated researchers contributing to this research are from the Singapore Institute of Manufacturing Technology and the Institute of Materials Research and Engineering.

28th of June 2017

References:

  1. Zhang, B., Bi, G., Wang, P, Bai, J., Chew, Y., & Nai, M. S. Microstructure and mechanical properties of Inconel 625/nano-TiB2 composite fabricated by LAAM. Materials & Design 11,70–79 (2016).| Article

Source: A*STAR Research

tribonet
About tribonet 313 Articles
Administration of the project

Be the first to comment

Leave a Reply

Your email address will not be published.


*


This site uses Akismet to reduce spam. Learn how your comment data is processed.