Friction Coefficients

09.02.2017 tribonet

Friction Coefficients of Solid Lubricants, Metals and Antifriction Materials Table of friction coefficients of various materials in atmosphere and vacuum (see the definition of friction coefficient). The data was collected from various sources [1,2,3]. Material […]