Graphene-Nanosheet
Atomistic Tribology

Controlling friction of graphene

Graphene, a wonder just one atom thick material, shows incredible wear-resistance and super low friction levels. This behavior is ascribed to its low inter-layer shear properties and high normal load carrying capabilities. However, in many […]