About TriboNet

Your guide to the world of tribology

What is TriboNet

An educational platform on tribology — the science of friction, wear and lubrication

Who is it for

Engineers, researchers, students and industry professionals

Topics

Friction, wear, lubricants, coatings, biotribology, nanotribology

Content formats

Wiki articles, webinars, videos, industry news, scientific reviews

Updates

Weekly news, regular webinars, continuous Wiki updates

Resources

500+ Wiki articles, webinar archive, company directory, event calendar

4 more points

Green Tribology

Green Tribology

Energy efficiency for future Electric vehicles

Introduction Achieving high energy efficiency is a primary objective for future Electric Vehicles (EVs) and Hybrid Electric Vehicles (HEVs). This is a goal which is closely intertwined with thermal efficiency and design considerations. Future research demands deeper exploration into lubricant...
Do Electric Vehicles Use Oil?
Green Tribology

Stribeck curve in Electric vehicle

Introduction Lubricants are integral to perform various functions in the vehicle components, significantly impacting overall performance. Electric vehicles (EVs) are mainly equipped with electric motors that typically exhibits higher acceleration rates compared to vehicles with mechanical engines. Consequently, lubricants in...
Green Tribology

Lubricants in Electric vehicles

Introduction The tribological requirements for Electric Vehicles (EVs) and Hybrid Electric Vehicles (HEVs) differ from those of Internal Combustion Engine (ICE) vehicles. In EVs, key concerns include a lubricant's thermal and electrical properties, copper corrosion, and compatibility with the elastomers/polymers...
Green Tribology

Tribological needs in Electric and hybrid electric vehicles

Introduction Mobility has long been a game-changer for humanity which traces back to the ancient invention of wheels. However, the real revolution began in 1769 with Nicolas Joseph Cugnot's steam-powered automobile which kicked off curiosity for fuel experimentation. Karl Benz's...
Sustainability in the Workplace: Why it Matters and What You Can Do - FMP Consulting
Green Tribology

Tackling Energy waste through Sustainable Tribology

In recent decades, the focus on sustainability has intensified among designers and tribologists, making energy conservation and sustainability as an important areas of research. In today's context, energy plays a central role in nearly every human activity, impacting various aspects...
A close-up of hands holding a pile of shredded paper Description automatically generated
Green Tribology

Unleashing the Hidden Potential of Recycled Plastics in Tribology – Part 2: Polypropylene

The problem with polypropylene recycling Polypropylene (PP; ♻️ 5) is all around us. It is found in diverse applications ranging from takeaway containers to car bumpers. Despite being one of the most produced polymers globally, PP lags behind in recycling....
A pile of colorful plastic caps Description automatically generated
Green Tribology

Unleashing the Hidden Potential of Recycled Plastics in Tribology – Part 1: Polyethylene

What happens to recycled plastic? Plastic recycling is great. It is everywhere. Or at least, the talk of it is everywhere. In places with good waste management infrastructure, separately discarded plastic waste goes through a system of sorting, shredding and...